1
Generic Aquasport Rebuilding Topics / Re: 1973 196 rebuild question
« Last post by Duffy1470 on Today at 04:00:46 PM »Also, picked up two sheets 3/4 in Coosa, 5 gal of poly resin, mek, bubble buster roller, roll of Matt, and got a roll of something heavier than 1708. The heavier stuff was a "good deal". We'll see. At any rate, going to patch holes in outer skin of transom first. Question, I know it's 11ccs of me for a quart of poly resin at 70 degrees Fahrenheit, less if hotter. How much less, say at 75, 80, 85 degrees. It's getting hot here 8n tn. Thanks.